Add to Cart
This is the printing paper which can be laminated into 2 pcs of the glass, and bond together by the EVA film.
The processing temperature we suggest is 90-115 degree, if the temperature is too high, the pattern will be damaged.
Processing details: Glass/EVA/paper/EVA/glass or you can laminate the sigle layer glass: glass/EVA/paper
=